> -----Original Message-----
> From: Louis, Edwin @ CSE
> Sent: Tuesday, April 01, 2003 9:06 AM
> To: [log in to unmask]
> Subject: FW: Gold PLating over Copper/or Nickel
>
>
>
> -----Original Message-----
> From: Louis, Edwin @ CSE
> Sent: Tuesday, April 01, 2003 9:01 AM
> To: [log in to unmask]
> Subject: Gold PLating over Copper/or Nickel
>
> WE have a situation where a vendor who is manufacturing a module for us
> can not seem to plate Nickel and Gold into blind vias.
> The vias are 30mils in diameter and 10 mils deep.If we don't get Nickel
> plated into the holes we may end up with bare Copper
> or Gold over bare Copper. Can one of you make comment on our situation.
> The Copper in a plate over Aluminum base metal.
> It seems to me that the vendor should be able to plate in the vias I
> mentioned with the aspect ratio given.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|