Carl,
It might be CEM1 or CEM3. This is a paper based material rather
than fiberglass.
Good Luck
On 25 Apr 03, at 8:04, Carl VanWormer wrote:
> I can contact the FR-4 laminate manufacturers, but I don't know what the tan
> material is that is used in PC power supplies, so I don't know who to
> contact . . .Any clues on what that stuff is?
>
>
>
>
>
> Carl Van Wormer
> Cipher Systems
> 1815 NW 169th Place, Suite 5010
> Beaverton, OR 97006
> Phone (503)-617-7447 Fax (503)-617-6550
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
> Sent: Friday, April 25, 2003 8:02 AM
> To: [log in to unmask]
> Subject: Re: [TN] PCB Material Question
>
>
> Carl,
>
> Perhaps the best way would be to just contact the major laminate supplies
> and ask
> them for data sheets on their lines of laminate.
>
> Larry ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Techne
t NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Dig
est
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
Peter Menuez
QA Manager
Proto Circuit, Inc.
330-572-3400
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|