Ken if you check out the paper in appendix 5 of 4552 you will see the data
on using ENIG as a switch pad material. Most applications I have seen HASL
and Carbon used for over the years are for soft touch membrane type switches
- ENIG is a definite replacement for these. If a rotary switch application
is being used then ENIG is the wrong finish.
Regards
Gerard O'Brien
Co-chairman 4552/4553/4554.............45XX
-----Original Message-----
From: Ken Patel [mailto:[log in to unmask]]
Sent: Tuesday, April 29, 2003 4:26 PM
To: [log in to unmask]
Subject: [TN] Surface Finish
Expert,
Can Carbon ink and HASL finish be replaced entirely by ENIG finish or any
other finish?
re,
ken patel
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|