This is not to overlook the FR4 Tan Laminate made many years ago ---- Maybe
still made on East Coast.
Bernie Kessler
At 05:12 PM 04/28/2003 +0100, you wrote:
>Carl,
>
>The tan laminate is more than likely to be either FR2 or FR3. Both are paper
>based, FR2 is phenolic resin, Fr3 is epoxy resin. The IPC references are:-
>FR2 = IPC 4101/03. FR3 = IPC 4101/04.
>
>BTW Doug,
>CEM1&3 aren't cyanate ester laminates. CEM 1 is a paper core with a woven
>glass surface bonded with phenolic resin.
>CEM3 is is a non-woven glass core with a woven glass surface bonded with
>epoxy resin.
>
>OK class over for the day. Time to get some Scottish Mountain Dew.
>
>Geoff Layhe
>
>
>
>
>-----Original Message-----
>From: [log in to unmask] [mailto:[log in to unmask]]
>Sent: Friday, April 25, 2003 4:40 PM
>To: [log in to unmask]
>Subject: Re: [TN] PCB Material Question
>
>
>Carl, the tan material you see is probably CEM-1 or CEM-3. CEM stands for
>Cyanate Ester - Modified. It is a low cost laminate that is more often
>punched than routed, and usually single sided. Never used in Class 3
>electronics (at least by smart people). Usually only class 1 stuff.
>
>?
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>-----------------------------------------------------
>
>
>Private & Confidential:
>This e-mail message is confidential and is intended solely for the person or
>organisation to whom it is addressed. If the message is received by anyone
>other than the addressee please return the message to the sender by replying
>to it and then delete the message from your computer.
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>-----------------------------------------------------
Bernard Kessler & Associates, Ltd
714-898-8422 562-598-5563 Fx: 562-431-1741
www.home.earthlink.net/~bkesslerbka
Service is our Profession
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|