Mr. Caswell,
Thanks for the info. I have not tried a water pick. May try this next.
What saponifier do you use? We use something called Ecosolve which works
great with our RMA flux. What type of flux are you using?
I may also try diverting a slip stream of the wash solution from our in-line
cleaner. Reduce the pressure and run it through some SS hose to drop the
temperature slightly.
thanks
joe
-----Original Message-----
From: Charles Caswell [mailto:[log in to unmask]]
Sent: Saturday, April 26, 2003 12:22 PM
To: [log in to unmask]
Subject: Re: [TN] cleaning under BGAs
Everybody has problems cleaning under BGA's. We bought an air powered
sprayer. We call it the car wash. The pickup hose just goes in the aqueous
tank. Works better than the Water Pik that we had been using. Got ours fr
McMaster Carr, about $100. Cat.# 5447K15. Pg. 1877 of my catalog. They have
others but do not get the brass nozzle, it does not like saponifier!
Charles caswell
The Big Kahuna
-----Original Message-----
From: Macko, Joe @ IEC [mailto:[log in to unmask]]
Sent: Saturday, April 26, 2003 12:57 PM
To: [log in to unmask]
Subject: [TN] cleaning under BGAs
Fellow Technets,
Periodically, BGAs are reflowed using our AIR-VAC hot air rework station.
RMA liquid flux is 1st flowed under the BGA prior to reflow and then clean
afterwards starting with IPA spray followed by an in-line cleaner wash.
Occasionally, flux residue remains which requires additional cleaning.
I am in need of a creative and operator safe way to either spray/flow warm
IPA or a mixture of hot saponifier/DI water (from our in-line cleaner) under
BGAs to expedite cleaning. I do not know of any equipment on the market
that can be used for this application.
Welcome ALL suggestions and proven methods. thanks
joe
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|