Just make sure you have adequate ventillation of the room, or do it
outdoors, that process stinks...bad...real bad
----- Original Message -----
From: "Crepeau, Phil" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, April 24, 2003 9:26 AM
Subject: Re: [TN] Warped boards
hi,
i agree with this conclusion. some time back we were getting boards that
warped to an hyperbolic paraboloid shape (you know; like a saddle). burning
out the resin showed that warp and fill directions of the glass cloth ran
one way in one layer and another in a second layer. those boards that
didn't warp had all warp and fill running in the same direction. this might
explain the sudden increase in warp problems with a vendor. so...burn out
the resin in a warped board and count the weave in each direction. do the
same with a non-warped board.
phil
-----Original Message-----
From: Franklin D Asbell [mailto:[log in to unmask]]
Sent: Thursday, April 24, 2003 6:27 AM
To: [log in to unmask]
Subject: Re: [TN] Warped boards
Sounds like to issues...
1) From your board description, with everything being balanced I am assuming
it is a multilayer board, when we see warpage in otherwise balanced layup it
often is cross-weave/ply in the prepreg, if this were the case there is
probably no way to remedy it, other than use as is...somehow...
2) Regarding meeting IPC requirements...the hard approach would be, did you
ask them to meet it? Yes? the you got what you asked for...now learn from
it... If they exceed the specification then you have a strong position...use
it to achieve a better product next time.
Often we recieve purchase order requirements from customers that are boxed,
or generic, and then when a condition may get to the customer they want to
reject for this condition, even though it is well within the "documented
requirements"...so what's a board shop to do...
The problem is often this...designers are sometimes unfamiliar with the IPC
requirements, but place them on drawings nonetheless, buyers are often even
more unfamiliar, and add these additional requirements to the purchase
order, it is only after the boards are received and processed that a company
learns they may have been to lax in some areas...i.e. bow and twist...and
the stuff hits the fan...
Even though the customer orders certain criteria does not necessarily mean
they can use that product (form-fit-function...etc etc) and bow and twist is
a fine example, especially with the tighter and tighter product emerging
(all you spec committess take note) the 1.5% and .75% may not be accurate
with some product...
Bottom line, it is up to the customer to be aware of what they are ordering,
or specifying, to the board shop, it is up to both the customer and board
shop to work towards a consensus on what is achieveable (in fabricating and
assembly) and write product specific specifications or tolerances...because
even if IPC updates the specification, this still will not cover all
eventuality...
In closing, we have also "battled" with customers in regards to warpage;
however, as part of these interesting discussions on meeting
specification -versus- meeting assembly or end use requirements we offer to
assist in revising product specific tolerances as well as give price
reduction, on occasion, for replacement boards in a good faith effort to
help them through this learning opportunity.
...okay, now that I'm behind in my work...I'll let you all ponder that...
Franklin
----- Original Message -----
From: "Grant Emandien" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, April 24, 2003 1:20 AM
Subject: [TN] Warped boards
> T'netters,
>
> On the matter of warped boards we are currently experiencing this problem
> (warpage appears to be in either direction i.e. to the solder or component
> side, sometimes exhibits and S-curve), - we do not bake these boards to
> remedy but rather reject and return, hence the stand-off with the pcb
> fabricator who is insistent that it is within acceptable IPC stds. PCB
> details are:
>
> * PCBs are approx. 300mm x 135mm in area,
> * made of std. Duraver E-Cu 104 (Tg of 135degC) from Isola (no
further
> details),
> * exhibits relatively good copper balance on both sides, only about
> 20% of the surface is coppe,.
> * is only exposed to wave solder heat - it appears that the wave
heat
> may also worsen the problem, so it may appear that stress is already
present
> (on good boards) in the material before wave.
>
> Any experience of this material, what the fabricator's process may be
> inducing and any other possible contributary factors?
>
> Advice graciously received, TIA
> Grant
>
>
> **********************************************************************
> Notice:
>
> This email transmission contains confidential information which is the
property of the
> sender and if you are not the intended recipient, you are hereby notified
that any
> disclosure, copying or distribution of the contents of this e-mail
transmission, or the
> taking of any action in reliance thereon or pursuant thereto, is strictly
prohibited.
> Should you have received this e-mail in error, please notify us
immediately to arrange
> for the return of the documentation comprising this transmission. No
warranty is given by
> Tellumat (Pty) Ltd regarding the integrity of this e-mail, nor that this
e-mail is free
> of viruses, interception or interference. Unless otherwise stated, any
views or opinions
> contained in this e-mail are that of the sender. Tellumat (Pty) Ltd
furthermore disclaims
> liability for any unauthorised opinion or representation made by the
sender purportedly
> on behalf of Tellumat (Pty) Ltd. Accordingly, Tellumat (Pty) Ltd's
delegation of
> authorities, setting out who may contract on behalf of Tellumat (Pty) Ltd,
is available
> on request to the recipient.
>
> **********************************************************************
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|