Should be doable. I believe Epotek
http://www.epotek.com/solder_replace.html is the epoxy vendor with the most
data.
-----Original Message-----
From: Dan R. Johnson [mailto:[log in to unmask]]
Sent: Wednesday, April 23, 2003 4:04 PM
To: [log in to unmask]
Subject: [TN] SOLDER/EPOXY REACTION
I have a customer who is trying to attach our SMT part to their hybrid
assembly using silver fill epoxy. We use a lead free alloy (Sn 96.5/Ag
3.5).
Any body have any experiences in this area. The customer (actually the CM)
is worried about dissimilar metals and long term reliability, should they?
Thanks,
Dan
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------