Look like poor plating...
jk
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Prashant Chopra
>Sent: Tuesday, April 22, 2003 2:59 AM
>To: [log in to unmask]
>Subject: [TN] problem with gold pads of the pcb
>
>
>hi all,
>
>we are using gold finger pads on the pcb. but after going thru
>smt process of screen printing,component insertion, reflow and
>aqueous wash we are facing the problem of grey color dots on the pads.
>
>This problem is with the pads where no components are being placed.
>
>There is no solder paste printing on these pads nor any
>components are place there and they are being covered with
>Kapton tape thru out the above process.
>
>
>Can anyone point to some reasons for this problem?????
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using
>LISTSERV 1.8e To unsubscribe, send a message to
>[log in to unmask] with following text in the BODY (NOT the
>subject field): SIGNOFF Technet To temporarily halt or
>(re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE
>mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest Search the archives of
>previous posts at: http://listserv.ipc.org/archives Please
>visit IPC web site http://www.ipc.org/html/forum.htm for
>additional information, or contact Keach Sasamori at
>[log in to unmask] or 847-509-9700 ext.5315
>-----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|