may i add a couple of other differences? thanks. pvc wire insulation cannot be used on military programs (it gives off a carcinogen when it burns).
teflon wire insulation has very poor cold flow, and should not be used where it might come into contact with sharp edges, corners, and points.
teflon insulation has very good dielectric properties.
teflon insulation is difficult to bond to unless you pull off a few fluorine atoms with sodium (read tetra etch).
Kynar wire insulation can be a good substitute for teflon when teflons shortcomings are difficult to live with.
phil
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------