TECHNET Archives

April 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
X-To:
Date:
Fri, 25 Apr 2003 09:58:44 -0400
Content-Disposition:
inline
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Collins Graham <[log in to unmask]>
Subject:
From:
Collins Graham <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Sender:
Parts/Attachments:
text/plain (147 lines)
gold leads.  It's a mil spec part, comes in with gold.

Charles - Why would you be sorry, I'm the one with the pain in the
$#@$#@!!! parts...

Ramon - the matrix tray is OK so long as the parts can't shift.  If the
tray is properly held together it's fine, but if there is any gap then
the parts can shift around.

 - Graham

regards,

Graham Collins
Process Engineer,
Northrop Grumman Canada Corporation
Halifax
(902) 873-2000 ext 6215

>>> [log in to unmask] 04/25/03 10:33AM >>>
I know I will be sorry for this. Why do the parts need to be tinned?
Charles

-----Original Message-----
From: Dehoyos, Ramon [mailto:[log in to unmask]]
Sent: Friday, April 25, 2003 8:09 AM
To: [log in to unmask]
Subject: Re: [TN] Velcro straps for matrix trays?


        Parts should not move and leads deform while in the box during
transportation. It seems that the parts because of the big size and
weight
are not properly package and allowed to shift and bend the leads.
Perhaps
packaging them in the proper container will eliminate the problem. The
proper container should barely touch the tip of lead toes but not the
bottom
of the feet and the cover should put pressure on the ceramic body when
closed.
        Regards,
        Ramon

> -----Original Message-----
> From: Collins Graham [SMTP:[log in to unmask]]
> Sent: Friday, April 25, 2003 7:01 AM
> To:   [log in to unmask]
> Subject:      Re: [TN] Velcro straps for matrix trays?
>
> Hi Eric, Brad, Arthur
> Thanks for the replies.
>
> Eric - An interesting observation, I've just blindly assumed that
the
> manufacturer of the components would supply them with an appropriate
ESD
> safe velcro strap.  A dangerous assumption perhaps.  But how
dangerous
> is it given that the tray is conductive, the bench is conductive,
and
> the operator putting on or removing the straps is grounded?
>
> The problem I've got is that these QFPs are big, ceramic, and have
> leads that behave as if they are made of butter.  They have to be
> received, inspected, tinned, inspected, and pick/placed - so a fair
bit
> of handling and examination.  Using elastic bands has been a
disaster,
> although my abilities to tweak leads with ax X-Acto knife are
improving
> as a result.   Using Kapton tape to secure the trays together has
not
> worked well either, it only takes marginal movement to allow the
parts
> to shift.  The only success I've had is using the big clamp type
paper
> clips, one can fasten two trays together with a clip on each end and
> there is no movement.  Not a really practical solution though.
>
> The velcro straps work wonderfully, but we only have a couple in
house.
>  Most of our matrix tray packed parts arrive ready to use, with heat
> sealed plastic bands holding them.  These don't get opened until we
are
> ready to use them.
>
> Thanks all, and have a good weekend.
>
> Oh, and Peter Duncan - I flipped a long time ago.  This is not new
> news.  Just trying to put a bit of humor into a forum that has gone
a
> bit dry...
>
>  - Graham Collins
> >  A mundane question for such a highly technical body, but
hopefully
>
> 1.8e
>

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV
1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV
1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2