Hi Dave,
With good solderability and well-designed landsize, distance between
land and soldermask, and soldermask-thickness you should get all of the
via's filled or at least capped. Optimizing this may be a better and
cheaper solution than via-filling at the bare board level.
An effective alternative solution could be to change the testprobes.
Consult your ICT-vendor to see what the options are.
Daan Terstegge
Thales Communications
Unclassified mail
Personal Website: http://www.smtinfo.net
>>> [log in to unmask] 04/15/03 01:09pm >>>
I do have a question and would like a response offline please. I have
2000
vias on the bottomside of a wave soldered board and vias (not all) will
be
used by test. Problem is operators spend way too long inspecting to see
the
vias are filled by the wave. I want to fill the vias with conductive
epoxy,
Methode or Dupont material. I hear it is done but can find none of our
board houses who have ever done it. Is this a fantasy? A good theory no
one
is doing? Why not? I got a response that it is "very very expensive"
what
does that mean? $1 a board more $10 a board more? And yes I have
searched
the archives. This is a high volume job I may be able to eliminate 3
shifts
worth of inspection vs. whatever the increased board cost is.
Thank you. I promise to post results to Steve's website complete with
pictures whether it works or not.
Dave Chapman
Manufacturing Engineer
Circuit Service Inc.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV
1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV
1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|