Hi, Genny,
My condolences! PVC-coated wire was banned from use in aircraft equipment
owing to its lack of flame retardant abilities. The PTFE-coated wire
family, of which Teflon is a member, was the preferred replacement.
I think you can infer when to use PVC and when not to - if, as a result of
your equipment catching fire, there is a likelihood of further endangering
life through increased flame or smoke, then don't use it.
Do you now need to change out the wire? Good luck!
Peter
Genny Gibbard <[log in to unmask]> 24/04/2003 03:46 AM
Sent by: TechNet <[log in to unmask]>
Please respond to "TechNet E-Mail Forum."; Please respond to Genny Gibbard
To: [log in to unmask]
cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Subject: [TN] wire coatings
Do you remember my question regarding the midplane assembly?
Turns out that there was a reel of mislabelled wire in house, and a whole
bunch of assembly has been done using a PVC coated wire, instead of the
teflon coated wire I spec'd. Apparently the wire in question is obsolete,
but they like using it better than the teflon, and want to continue to use
that.
I don't know much about wire coatings - what is the difference between
these
two coating types, and when would you want to or not want to use them. I
need to decide whether we need to force them to change out the wiring
they've already done.
Sigh...
Thanks for your help in advance.
Genny Gibbard (mailto:[log in to unmask])
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|