TECHNET Archives

April 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"Dehoyos, Ramon" <[log in to unmask]>
Date:
Tue, 8 Apr 2003 05:43:29 -0700
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (89 lines)
        Have you tried top fluxing?   Yes, preheating a thick board in an
oven improves the solder  flow to the top, making sure that the boards go
from the oven to the wave without cooling off.
        Regards,
        Ramon



> -----Original Message-----
> From: Steve Gregory [SMTP:[log in to unmask]]
> Sent: Monday, April 07, 2003 10:36 PM
> To:   [log in to unmask]
> Subject:      Re: [TN] Wave soldering - Spray fluxer parameters
>
> Hi Peter!
>
> Not knowing what type of spray-fluxer you have, I'll tell you what I do
> here with the Opti-flux system I have...it's a ultra-sonic fluxer.
>
> What I look for is coverage first of all. That's easily checked by either
> using a piece of cardboard, or with kraft paper taped to the fixture
> you're using, that corresponds to the width of the conveyer. Then just run
> it through the fluxer with the heaters off. Take a look at the spray
> pattern and look for even coverage.
>
> With my spray fluxer I can adjust what's called the traverse speed, which
> controls how fast the spray head passes back and forth. If I run the main
> conveyor speed a little fast, I may need to increase the spray fluxer
> traverse speed so that there's even coverage...it's always worked for me.
>
> That being said, I'm running into a challenge with a big, thick (.125"),
> heavy back-plane that I'm trying to wave. It's a class-3 assembly, and
> having a hard time getting good top-side fillets. Gonna try pre-heating
> the assembly in a oven, taking it out and getting it into the wave before
> it has a chance to cool down a whole lot. I've tried playing with
> pre-heat, conveyer speed, etc...but it seems everything that I try to do
> on the wave, seems to dry-out, or kill the flux...
>
> Maybe someone has another suggestion...BTW, I have an Electrovert Electra.
>
> -Steve Gregory-
>
>
>
>       Technet,
>
>       Can anyone recommend a process for setting up the operating
> parameters
>       for the spray fluxer?
>
>       How can one verify the optimum amount of flux is being applied to
> the
>       pcb prior to the board going through solder wave?
>
>
>       Rgds,
>       Peter
>
>
>
>
>
> -Steve Gregory-
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2