TECHNET Archives

April 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Gaugler, Kevin" <[log in to unmask]>
Date:
Wed, 30 Apr 2003 12:17:57 +0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=us-ascii
Subject:
From:
X-cc:
MIME-Version:
1.0
Parts/Attachments:
text/plain (125 lines)
Coke as a rust-reducer, huh? Never thought of sharing a coke with my old
cars!

Peter



"Gaugler, Kevin" <[log in to unmask]>   30/04/2003 12:11 AM
Sent by: TechNet <[log in to unmask]>

Please respond to "TechNet E-Mail Forum."; Please respond to "Gaugler,
Kevin"

              To:  [log in to unmask]
              cc:  (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
              Subject: Re: [TN] Brominated Hydrocarbons and Mountain Dew (NTC-sort of)








Hi Mike,

Brominated vegetable oil is used as an emulsifying agent.  As far as I
know, you can't use it in the EU or in Canada because it is believed to be
a carcinogen.  Man, I know now that I am sticking with Coke (not quite as
much caffeine, but it's got Phosphoric acid!)

Regards,

Kevin Gaugler
      -----Original Message-----
      From: Mcmaster, Michael [mailto:[log in to unmask]]
      Sent: Tuesday, April 29, 2003 11:57 AM
      To: [log in to unmask]
      Subject: [TN] Brominated Hydrocarbons and Mountain Dew (NTC-sort of)



      This posting has no relevance to circuit boards or assemblies, but
      given the amount of discussion on this forum on the drive to
      eliminate brominated flame retardants in PWB materials and the
      fondness of some regulars for the Dew, I think it's relevant.


      The other day, I noticed one of my co-workers drinking a liquid that
      was unnaturally bright red.  I queried him on exactly what this
      liquid was.  He replied Mountain Dew Code Red.  This led to a
      discussion of what exactly was Code Red.  A scan of the ingredients
      revealed the expected red dye but surprisingly, it also contained
      brominated vegetable oil.  I immediately asked why the makers of this
      product felt it necessary to add an apparent flame retardant to their
      product.  My co-worker (incidentally a chemist who really should no
      better but claims that he somehow manages to compartmentalize all
      this stuff) had no idea.


      I just thought this whole thing is very ironic.  Most of us work in
      an industry that is spending millions of dollars trying to remove
      bromine from one of the constituents while at the same time you have
      a "food" product to which intentionally is added a brominated
      hydrocarbon. Does anybody know what purpose the brominated vegetable
      oil serves? It also turns out the some component is in regular Dew as
      well as diet red dew but not diet regular Dew.


      Now back to our regularly scheduled programming....
      Mike McMaster
      RF Product Engineer
      Merix Corporation
      503-992-4263




      ---------------------------------------------------
      Technet Mail List provided as a free service by IPC using LISTSERV
      1.8e
      To unsubscribe, send a message to [log in to unmask] with following
      text in the BODY (NOT the subject field): SIGNOFF Technet
      To temporarily halt or (re-start) delivery of Technet send e-mail to
      [log in to unmask]: SET Technet NOMAIL or (MAIL)
      To receive ONE mailing per day of all the posts: send e-mail to
      [log in to unmask]: SET Technet Digest
      Search the archives of previous posts at:
      http://listserv.ipc.org/archives
      Please visit IPC web site http://www.ipc.org/html/forum.htm for
      additional information, or contact Keach Sasamori at [log in to unmask]
      or 847-509-9700 ext.5315
      -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------



[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2