Hi Brian,
Can you inform what are your packaging mentioned parameters for 15 years?
Best Regards
ROKAH Reuven
Brian Ellis
<b_ellis@PROTONI To: [log in to unmask]
QUE.COM> cc:
Sent by: TechNet Subject: Re: [TN] Expiry time in vacuum package
<[log in to unmask]
>
27/04/03 01:38
PM
Please respond
to "TechNet
E-Mail Forum.";
Please respond
to Brian Ellis
Sorry, still not good enough. What kind of vacuum package? How thick?
How sealed? What vacuum? What conditions of storage? What component
construction? What finish? How clean? How do you define
reliability/functionality? What figure of confidence level? How long is
a piece of string?
Brian
Reuven ROKAH wrote:
> Hi Brian
>
> How long active component (BGA, QFP, SOP) or finish product (assembled
PCB
> - finish good) can be stored in a sealed / vacuum package and still
having
> confidence with its reliability / functionality in its system.
>
> Best Regards
>
> ROKAH Reuven
>
>
>
>
> Brian Ellis
> <b_ellis@PROTONI To: [log in to unmask]
> QUE.COM> cc:
> Sent by: TechNet Subject: Re: [TN] Expiry
time in vacuum package
> <[log in to unmask]
> >
>
>
> 27/04/03 12:06
> PM
> Please respond
> to "TechNet
> E-Mail Forum.";
> Please respond
> to Brian Ellis
>
>
>
>
>
> Uh? How long is a piece of string? Please be more precise
>
> Brian
>
> Reuven ROKAH wrote:
>
>>Hello Technet forum,
>>
>>Pls reply how long Active component of assembled PCB / system can be
>
> stored
>
>>in sealed / vacuum package before use / operating the system / component.
>>
>>
>>Best Regards
>>
>>ROKAH Reuven
>>
>>---------------------------------------------------
>>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>>To unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet
>>To temporarily halt or (re-start) delivery of Technet send e-mail to
>
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>
>>To receive ONE mailing per day of all the posts: send e-mail to
>
> [log in to unmask]: SET Technet Digest
>
>>Search the archives of previous posts at:
>
> http://listserv.ipc.org/archives
>
>>Please visit IPC web site http://www.ipc.org/html/forum.htm for
>
> additional
>
>>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>
> ext.5315
>
>>-----------------------------------------------------
>>
>>
>>
>>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
>
>
>
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|