Sherif,
Check for "foreign inclusions" and contamination. If your circuitry is exposed to
high humidity and temperature swings delamination will result if there is
forgein material.
David A. Douthit
Manager
LoCan LLC
Sherif Refaat wrote:
> Hi Bill,
>
> Per IPC-A-600, Par. 3.1.1. for boards class 2 and 3 the nonconforming voids
> are described as "Voids in excess of 0.08 mm (0.003 in) or voids violate
> minimum dielectric spacing". The same requirements are also found in
> IPC-6012A Par. 3.6.2.3.
>
> I'm in the midst of a problem that, I believe, has to do with laminate
> voids. The assembled boards are failing in the field after few weeks to
> several months of service!! These modules are not for high altitude
> application. The voids occurred in a laminated core (so it is a laminate
> supplier problem not PCBs manufacturer problem) between power and ground
> layers.
>
> Sherif,
>
> ----- Original Message -----
> From: "Brown, William G" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Tuesday, April 22, 2003 1:45 PM
> Subject: [TN] Voids / Air Pockets in Laminates
>
> > Hi All,
> >
> > Does anyone know where I can find information on air bubbles or voids
> within
> > completed circuit boards? We have a group here which is concerned about
> any
> > voids left when the laminates are pressed together, either within or
> between
> > layers, and the effects they might have at high altitudes.
> >
> > Are there any IPC specs which state allowable values or anything like
> that?
> > These are boards made with IPC-4101/ 40, 41 or 42 materials.
> >
> > Thanks for any help!
> > Bill
> >
> > ############################################
> > William G. Brown
> > Senior Electrical Engineer - PWD Engineering Support
> > > xBAE SYSTEMSx - Information & Electronic Warfare Systems
> > Phone: 603-885-4930 Fax: 603-885-5435
> > ############################################
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following text in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at: http://listserv.ipc.org/archives
> > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> > -----------------------------------------------------
> >
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|