Hi and Welcome Angela! Contact any of the solder material suppliers (e.g.
Kester, Alpha, Indium, etc.) - and request information about their solder
preform products. Solder donuts or "solder preforms" can be furnished in a
wide variety of dimensions. It is also not uncommon to have custom preforms
created to fit your specific application (note, everything comes with a
cost!). Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Angela Gregor
<agregor@symetric To: [log in to unmask]
s.com> cc:
Sent by: TechNet Subject: [TN] Controlled Solder
<[log in to unmask]>
04/17/2003 12:44
PM
Please respond to
agregor
Hello everyone! As a new member I am going to put this new tool to the test
immediately. I work for a small company in Florida, and we build mainly
defense product for the government. We have a big problem hopefully someone
can help with. We are currently building a product that has through hole
cylindrical type hollow pins inserted into a printed circuit board then
soldered into place. (solder is not allowed to make contact with the inside
wall of the hollow pins). We are allowed only minimal amount of solder. It
is extremely difficult to achieve this while maintaining 75% fill of solder
in the board. I have heard of something called solder doughnuts that will
allow us to flow the same amount of solder each time but have been
unsuccessful in locating them. Any advise would be helpful. Thanks! Angela
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|