What does the strain gage test result measure against? Is it the tensile
strength of the specimen?
and how does that comparison work? (how to interpret the result from the
test?)
(I am about to hire someone from outside to perform astrain gage test to see
if there is any correlation between ICT fixture and a cracked trace found
near a ICT probe. )
----------------------------------------------------------------------------
--------------------------------------------------------------------------
What is the most common, or grade 1 copper foil in terms of the copper class
and type per IPC CF-152?
There are Type E class 1, 2, 3, and 4. and
There are Type W class 5,6,7 and 8.
Which one of this is considered as grade 1 material?
Thanks for reading.
Rudolph Yu
NPI Engineer
Adaptec, Inc.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|