Siggi,
There has already been one reliability "disaster" using Phosphor
as a bromide replacement in molding compounds.
This one is still being painfully felt around the world.
David A. Douthit
Manager
LoCan LLC
"Zweigart, Siegmund" wrote:
> Yes the bromide will be not allowed any more, but it will be replaced by
> Phosphor, therefore the FR can still alive.
>
> Siggi
>
> -----Original Message-----
> From: d. terstegge [mailto:[log in to unmask]]
> Sent: Mittwoch, 16. April 2003 09:17
> To: [log in to unmask]
> Subject: Re: [TN] Halogen-free No-flow Materials
>
> I sure hope so, because (to my knowledge) the bromide based flame
> retardents fall under the same EC-directives that forbid the use of lead
> in electronic products by 2006.
>
> Daan Terstegge
> Thales Communications
> Unclassified mail
> Personal Website: http://www.smtinfo.net
>
> >>> [log in to unmask] 04/16/03 03:58am >>>
> Mike,
>
> This should be interesting since the "FR" in FR stands for "Flame
> Retardent".
> Bromide compounds are the flame retardents. Let's see if anyone has
> developed a halogen-free FR material.
>
> David A. Douthit
> Manager
> LoCan LLC
>
> "Mcmaster, Michael" wrote:
>
> >
> >
> > I'm hoping that there are at least a few laminate manufacturers
> among
> > the 800 or so remaining subscribers.
> >
> > I'm looking for a no- or controlled-flow prepreg that will qualify
> as
> > halogen-free. Preferably FR4-type but I'll consider other
> materials.
> > If anyone has any recommendations I'd like to hear about it. Feel
> > free to contact me off-line if you're a material supplier and fear
> > recriminations for being too capitalistic ;-).
> >
> > Mike McMaster
> > RF Product Engineer
> > Merix Corporation
> > 503-992-4263
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a free service by IPC using LISTSERV
> > 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following
> text
> > in the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at:
> > http://listserv.ipc.org/archives
> > Please visit IPC web site http://www.ipc.org/html/forum.htm for
> > additional information, or contact Keach Sasamori at [log in to unmask]
> or
> > 847-509-9700 ext.5315
> > -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV
> 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|