TECHNET Archives

April 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 16 Apr 2003 09:49:27 +0200
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Zweigart, Siegmund" <[log in to unmask]>
Subject:
From:
"Zweigart, Siegmund" <[log in to unmask]>
X-cc:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (181 lines)
It was not my thought, just what I heard from the PCB makers

Siggi

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Mittwoch, 16. April 2003 09:44
To: TechNet E-Mail Forum.; Zweigart, Siegmund
Cc: [log in to unmask]
Subject: Re: [TN] Halogen-free No-flow Materials



Phosphor, eh? That means  if ever any of my avionics boards burn, they will
have a secondary function as distress flares, thereby saving the weight of
flares and flare guns in the aircraft. Good thought!

Peter


"Zweigart, Siegmund" <[log in to unmask]>    16/04/2003 03:27 PM
Sent by: TechNet <[log in to unmask]>

Please respond to "TechNet E-Mail Forum."; Please respond to "Zweigart,
Siegmund"


              To:  [log in to unmask]

              cc:  (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)

              Subject: Re: [TN] Halogen-free No-flow Materials












Yes the bromide will be not allowed any more, but it will be replaced by
Phosphor, therefore the FR can still alive.

Siggi

-----Original Message-----
From: d. terstegge [mailto:[log in to unmask]]
Sent: Mittwoch, 16. April 2003 09:17
To: [log in to unmask]
Subject: Re: [TN] Halogen-free No-flow Materials


I sure hope so, because (to my knowledge) the bromide based flame
retardents fall under the same EC-directives that forbid the use of lead
in electronic products by 2006.

Daan Terstegge
Thales Communications
Unclassified mail
Personal Website: http://www.smtinfo.net

>>> [log in to unmask] 04/16/03 03:58am >>>
Mike,

This should be interesting since the "FR" in FR stands for "Flame
Retardent".
Bromide compounds are the flame retardents. Let's see if anyone has
developed a halogen-free FR material.

David A. Douthit
Manager
LoCan LLC

"Mcmaster, Michael" wrote:

>
>
> I'm hoping that there are at least a few laminate manufacturers
among
> the 800 or so remaining subscribers.
>
> I'm looking for a no- or controlled-flow prepreg that will qualify
as
> halogen-free.  Preferably FR4-type but I'll consider other
materials.
> If anyone has any recommendations I'd like to hear about it.  Feel
> free to contact me off-line if you're a material supplier and fear
> recriminations for being too capitalistic ;-).
>
> Mike McMaster
> RF Product Engineer
> Merix Corporation
> 503-992-4263
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV
> 1.8e
> To unsubscribe, send a message to [log in to unmask] with following
text
> in the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
> additional information, or contact Keach Sasamori at [log in to unmask]
or
> 847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV
1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------




[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2