Ofer,
More than likely it's a storage problem. A combination of temperature and humidity changes
can distort plastic. This will be amplified if the components are stored "loose" ( not in seperate containers).
David A. Douthit
Manager
LoCan LLC
Ofer Cohen wrote:
> Good morning (strange to write it to global forum, but this is the hour
> here), technetters,
>
> I received a batch of bent component (BGA, plastic basis and metal cover).
> While placing it ion a test table the co-planarity error for this 32 mm
> component is 0.5 mm. Undoubtedly, can't be placed. Although we earned it
> (age - 3 years, storage conditions - unknown because procured from a
> jobber), I want to learn the possible cause for such a strange phenomena.
> Does anyone have an idea how it can happen?
>
> Regards
> Ofer Cohen
> Quality Assurance Manager
> Seabridge Ltd.
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|