TECHNET Archives

April 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Mon, 14 Apr 2003 16:27:57 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, John Parsons <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
John Parsons <[log in to unmask]>
Parts/Attachments:
text/plain (26 lines)
Greetings all,

I am looking for ideas on an effective means of changing the date/lot code
on phototools using some sort of labeling system.  The majority of our jobs
utilize a "lazy-8" style of marking for date and lot codes plotted directly
on the film but some of our older jobs which we do not have digital data for
rely on marking the phototool.  We have been using a Kroy Duratype 244
machine for many years for this purpose but it has recently come to my
attention that the quality of the labeling cartridge is not what it used to
be and the type is no longer dense enough to do the job.  Are there any
alternatives that you can recommend?

Regards
John Parsons

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2