Grant,
It can be done, but I wouldn't recommend doing it yourself, unless you really know what you are doing. There are legit companies out there that do this sort of thing that Lucent and Nortel use after fires, floods, etc. in major switching locations. I'll see if I can find some old contacts for you.
Bev Christian
Research in Motion
-----Original Message-----
From: Ofer Cohen [mailto:[log in to unmask]]
Sent: March 26, 2003 9:51 AM
To: [log in to unmask]
Subject: Re: [TN] Smoke damage to electronic assemblies
Grant,
Smoke is:
* in the short term - cause resistive bridging of electric circuit,
and
* in the long term - highly corrosive.
The cleaning is very complicated, as it is also sticky. If you can - trash
them. Otherwise - clean thoroughly with:
* first - solvents (IPA, etc.), then
* with detergent, then
* rinse, then
* check cleanliness,
* check thoroughly, including re-calibration.
If it is a product then its reliability will be low - let your customer know
(he will smell it anyway).
Regards
Ofer Cohen
Quality Assurance Manager
Seabridge Ltd.
-----Original Message-----
From: Grant Emandien [mailto:[log in to unmask]]
Sent: Wednesday, March 26, 2003 4:09 PM
To: [log in to unmask]
Subject: [TN] Smoke damage to electronic assemblies
'netters,
Can anyone offer advice on how to deal with smoke damaged assemblies wrt
possible damage and effects on reliability? Should it be trashed, cleaned up
etc? It appears that there may not have been any direct exposure to fire or
heat but certainly to smoke.
TIA
Grant
**********************************************************************
Notice:
This email transmission contains confidential information which is the
property of the
sender and if you are not the intended recipient, you are hereby notified
that any
disclosure, copying or distribution of the contents of this e-mail
transmission, or the
taking of any action in reliance thereon or pursuant thereto, is strictly
prohibited.
Should you have received this e-mail in error, please notify us immediately
to arrange
for the return of the documentation comprising this transmission. No
warranty is given by
Tellumat (Pty) Ltd regarding the integrity of this e-mail, nor that this
e-mail is free
of viruses, interception or interference. Unless otherwise stated, any views
or opinions
contained in this e-mail are that of the sender. Tellumat (Pty) Ltd
furthermore disclaims
liability for any unauthorised opinion or representation made by the sender
purportedly
on behalf of Tellumat (Pty) Ltd. Accordingly, Tellumat (Pty) Ltd's
delegation of
authorities, setting out who may contract on behalf of Tellumat (Pty) Ltd,
is available
on request to the recipient.
**********************************************************************
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|