Good point. There's not much exposed aluminum on a sub believe it or not, mostly steel, brass, bronze, stainless steel, other alloys. I imagine there's quite a lot of Al on a typical aircraft though.
Question: Does mercury vapor have the corrosive effect on aluminum, or just liquid Hg?
Best Regards,
Timothy Reeves
Technical Service Engineer - Matsushita Electronic Materials, Inc.
4114 Heather Street, Forest Grove, Oregon, 97116
Main (503) 357-8695 Direct (503) 992-5109 Cell (503) 781-1495 Fax (503) 357-8868
-----Original Message-----
From: David Douthit [mailto:[log in to unmask]]
Sent: Friday, March 21, 2003 10:17 AM
To: TechNet E-Mail Forum.; Tim Reeves
Subject: Re: [TN] Mercury Free Cert
Mercury will corrode aluminum at warp speed!!
David A. Douthit
Manager
LoCan LLC
Tim Reeves wrote:
> I think it's not so much that it's pressurized, actually atmospheric pressure in a submarine is on the low side (I served on one from 1988-92) but that it's enclosed with a recirculated atmosphere. In a submarine, oxygen is replenished, CO2 is scrubbed out and CO and hydrocarbons are oxidized, but certain contaminants are harder to remove.
> Mercury vaporizes enough to be a concern under standard conditions, and normally things vaporize more as the pressure is lowered.
> But you're right that it's not too surprising to receive a request for mercury-free certification.
>
> Best Regards,
> Timothy Reeves
> Technical Service Engineer - Matsushita Electronic Materials, Inc.
> 4114 Heather Street, Forest Grove, Oregon, 97116
> Main (503) 357-8695 Direct (503) 992-5109 Cell (503) 781-1495 Fax (503) 357-8868
>
> -----Original Message-----
> From: Quality [mailto:[log in to unmask]]
> Sent: Thursday, March 20, 2003 1:40 PM
> Subject: Re: Mercury Free Cert
>
> Mark,
>
> This is a fairly common request - especially for product that is
> going into a pressurized vessel. (Submarines, airplanes etc.)
> Seems mercury has a nasty habit of vaporizing under pressure.
>
> Anyway, we went through the effort a few years ago to assure no
> mercury is used in any materials we use - there were none. What
> you have to watch for is the use of things that contain mercury like
> thermometers.
>
> pete
> [log in to unmask]
>
> On 18 Mar 03, at 7:46, Mark Hargreaves wrote:
>
> > Hi All,
> > Seems to be my month for receiving unusual certification requests from our
> > bare board customers.
> >
> > Yesterday, a customer asked us to certify that our boards (or is it our
> > processes?) are "mercury free".
> >
> > Before I start sifting through MSDS's, is anyone aware of any PCB materials
> > (FR4), chemistries or processes that typically contain mercury?
> >
> > Are there any good info sources out there regarding mercury & PC fab?
> >
> > Many thanks for your responses to all of my past questions.
> >
> > Mark Hargreaves
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following text in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at: http://listserv.ipc.org/archives
> > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> > -----------------------------------------------------
>
> Peter Menuez
> QA Manager
> Proto Circuit, Inc.
> 330-572-3400
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|