I think a good test would be HALT/HASS (Highly Accelerated Life Test/Highly
Accelerated Stress Screening). This will push assemblies to failure and
tell you if possible flux residues are a major weak point in the product.
Difficult and cryptic to interpret but faster than traditional life testing.
Brad Vanderhoof
AITI
----- Original Message -----
From: "Bloomquist, Ken" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, March 20, 2003 1:42 PM
Subject: [TN] Flux Contamination Testing
> I have a question regarding a test for flux contamination on conformally
> coated boards.
>
> I know all about testing uncoated boards but was wondering if there are
any
> tests for type UR coated boards?
>
> Does a temperature soak do any good at bringing problems to the surface?
>
> Does baking cause any remaining flux to become conductive?
>
> Does a humidity/temperature soak do any good?
>
> What were looking for is a parallel electrical path that might reduce the
> value of a small SMT resistor.
>
> Thanks in advance,
>
> KennyB
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|