Dymax and Loctite each make a line of 1 and 2 part adhesives for bonding
ferrites.

Dave Fish
----- Original Message -----
From: "Shoda, Steve" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, March 20, 2003 5:00 PM
Subject: [TN] Adhesive bonding for ferrite cores


> Does anyone have any experience bonding ferrite cores?  I am working on
> developing a process for bonding an e-core to an i-core. They are 0.8" x
> 1.2" and sandwich the winding in the pwb. So the bond must be done once
the
> assembly is populated.   I'm applying a high viscosity epoxy, but it can
be
> difficult to control.  I attempted a 0.002" epoxy preform, but the outcome
> was reduced inductance, so we are still using the high viscosity epoxy.
Why
> would they result in such different inductance properties?   In either
case,
> the cure time at 250°F is 1 hour and production is requesting a material
> which has a very short cycle time.
>
> Steve Shoda
> BAE SYSTEMS Controls
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2