Hi Dave,
Hope you enjoyed the doughnut, I'm sipping bad coffee with sweet and low :(
A question about the filters you mentioned. We use alloy 770 and 752 for our
Rf Shields, I have never seen a solderability issue.
Even stock that was over five years old soldered great. What causes poor
solderability with the filters? Is it a "second pass" phenomena?
Dan
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------