Subject: | |
From: | |
Reply To: | TechNet E-Mail Forum. |
Date: | Mon, 3 Mar 2003 05:25:37 -0600 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
You can try Fancort. I purchased a "nibbler" from them a few years ago, worked pretty well.
http://www.fancort.com/
Royce
***********************************************************************
Royce Taylor
Process Engineering
Suntron Corporation NEO
104 Glenn Street
Lawrence, MA 01843
(978) 747-2061 voice
(978) 747-2010 fax
[log in to unmask]
www.suntroncorp.com
-----Original Message-----
From: Macko, Joe @ IEC [mailto:[log in to unmask]]
Sent: Friday, February 28, 2003 6:51 PM
To: [log in to unmask]
Subject: Re: [TN] Depaneling Tools
We also have odd formed boards that very in thickness from 062 to .100" The
boards are double sided with up to 12 layers. Automated, programmable
routers are nice but pricey and are volumes are low so your option sounds
interesting. Who are some of the distributors for Hepco's claw? thanks
joe
-----Original Message-----
From: Carl VanWormer [mailto:[log in to unmask]]
Sent: Friday, February 28, 2003 1:40 PM
To: [log in to unmask]
Subject: Re: [TN] Depaneling Tools
I have a Hepco 1.5mm "claw" that works well for low volume separation of
boards milled with an 0.062 bit. It's much better than snapping them apart!
I think it cost me about $20.
Carl Van Wormer
Cipher Systems
1815 NW 169th Place, Suite 5010
Beaverton, OR 97006
Phone (503)-617-7447 Fax (503)-617-6550
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Rich Lasko
Sent: Friday, February 28, 2003 1:34 PM
To: [log in to unmask]
Subject: [TN] Depaneling Tools
Good afternoon everyone,
I am looking for some information on some manual depaneling tools. I have
an assembly that has the array borders routed with "breakaway tabs".
However, during the depaneling process the operator basically bends the
array border back and forth to "snap" off the border. Hepco makes a
depaneling "claw" but I have not seen it in action. Any other thoughts on
depaneling tools?
Rich Lasko
Badger Electronics
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|