How quickly does gold tarnish? If you're lucky enough to find a gold nugget,
just think as you bank it that it has actually been knocking around the
planet for a few million years in all sorts of conditions and still is
bright and shiny, so I guess it will be OK on edge connectors:)
The underlying metals are possibly a concern in this context but you are
still looking at years.
Major concerns in a few weeks timescale therefore are, not tarnish, but
possible surface contamination (grease from handling and such like.)
Regards
Mike Fenner
Applications Engineer, European Operations
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Leadfree: www.Pb-Free.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Steve MacDonald
Sent: Tuesday, March 11, 2003 3:55 PM
To: [log in to unmask]
Subject: [TN] Gold Tarnish.
Greetings Mighty Techneters.
Under normal environmental conditions, (As in no special effort is being
made to create and maintain a particular controlled environment) how long
will it take for Gold (gold fingers) to tarnish or show evidence of
oxidation?
I am not considering any extremes in temperature and or humidity. Just on a
shelf at an assembly house.
I know how to clean them up, but someone asked me and I didn't have any
range of responses to offer.
Thank you,
Steve M.
---------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|