Hi Poh! This is one of those occasion's when both numbers are correct! The
"true" tin/lead eutectic composition is 61.9% tin and 38.1% Pb with a
melting temperature of 183C. The addition of silver lowers the melting
temperature slightly - Sn62/Pb36/Ag2 alloy is a near eutectic alloy with a
melting range of 177C-189C. Additionally the Sn63/Pb37 alloy is a near
eutectic alloy with a melting range of 183-187C. Solder alloy surface
tension also plays a role in tombstoning. Take a look at the Technet
archives - there was a lengthy discussion of the tombstone/solder alloy
topic some time ago.
Dave Hillman
Rockwell Collins
[log in to unmask]
Poh Kong Hui
<[log in to unmask] To: [log in to unmask]
M.SG> cc:
Sent by: TechNet Subject: [TN] Solder Paste with 0.4% silver
<[log in to unmask]>
03/22/2003 05:50
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to Poh
Kong Hui
Hi Technetters,
I understand that the 'anti-tombstone' solder paste contained 0.4% silver.
Some people told me that the melting point is 179 deg.C and other said it
was 183 deg.C.
I am wandering which is correct.
And what about the percentage for the tin & lead, whether the tin makes up
63% of the alloy & the lead consists of 1.6%, or some other number.
Thanks.
Regards,
Poh
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|