TECHNET Archives

March 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Tom Parkinson - Quality System Manager - WinTronics, Inc." <[log in to unmask]>
Date:
Tue, 11 Mar 2003 11:47:57 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Phil Nutting <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Phil Nutting <[log in to unmask]>
Parts/Attachments:
text/plain (66 lines)
Tom,

I agree with you.

Phil

-----Original Message-----
From: Tom Parkinson - Quality System Manager - WinTronics, Inc.
[mailto:[log in to unmask]]
Sent: Tuesday, March 11, 2003 11:39 AM
To: [log in to unmask]
Subject: Re: [TN] Mixing fluxes - more


I've read the recent questions and information concerning mixing of
fluxes.  I agree - do not mix flux types when soldering.  However,
here's one for you that can be looked at from a couple of angles....

1. I build a board - wave solder using washable flux.  Flux is
activated, does it's thing, and board is soldered.
2. Water Wash and Dry the board. All washable flux residue is gone.
3. Add a couple of more components that CANNOT be washed (water will
enter the component and ruin it), using NO-CLEAN.
4. Board is done.

Technically, I have used 2 types of fluxes on one assembly....

Another scenario:
1. Board (described above) is finished.  But, fails test - I find a bad
component...
2. I have to use NO CLEAN to replace the component because I cannot
water wash the board (remember the other components that cannot be
subjected to water wash..)
3. Board is done. Passes test - finished.

Again - Technically, I have mixed fluxes on the same assembly.

In the above description, I do not see a problem - or am I missing
something?


Thanks,
Tom

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2