TCE above Tg is non-linear. What you're asking for is like asking for
the distortion characteristics of a amp is after clipping.
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Arbour, Michel
> Sent: Friday, March 21, 2003 2:52 PM
> To: [log in to unmask]
> Subject: [TN] TCE above Tg for Dupont CB100 silver resin
>
>
> Hello Techies,
> By any chance, would you know what is the TCE > Tg
> for Dupont CB100 silver resin ??
>
> Can't get that info from DuPont's Micro-Circuit
> Materials group in the U.S. . They have not measured that
> characteristic they said...
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------