Here is the what Perfag specifies about board thickness (Perfag is a
specification for PCB, commonly used by PCB manufacturers) :
"The thickness tolerance is +-10%.
The thickness should be measured as follows :
a. by the PCB manufacturer :
just after lamination, i.e. including the copper foil of the outer layers
b. by the customer :
if possible over edge connector terminals, otherwise over clean-etched
laminate, adding the nominal thichness of the outer layers' copper foils and
substracting the nominal thickness of any masks.
Design note :
On plug-in boards, the clearance in the guide rails should be ensured with
respect to the total thickness of the board, possibly by withdrawng any
solder masks from the board edges.
In case where finished copper thickness is considered critical, the customer
should consult the PCB manufacturer."
Marie Magnin
FIRSTEC SA
Rue du Grand Pré 70
CH 1211 Genève 2
Tél. : +41(0)22 918 36 85
Fax : +41(0)22 918 36 93
mailto:[log in to unmask]
http://www.firstec.ch
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Franklin D Asbell
> Sent: lundi, 3. mars 2003 15:49
> To: [log in to unmask]
> Subject: [TN] PC Board thickness measurement
>
>
> In what IPC specification is board thickness measurement (location)
> referenced?
>
> I'm looking for where overall thickness is mentioned. I'm receiving
> conflicting information on whether the required board
> thickness is to be
> measured over foil copper (multilayer, after layup), over
> soldermask/glass,
> or over final finish.
>
> And is there information differentiating between OSP or flat
> coatings and
> HASL or reflow if final thickness is measured over...final finish...
>
> Thanks.
>
> Franklin
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using
> LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with
> following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send
> e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail
> to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm
> for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|