As requested an online reply
95.5Sn/3.9Ag/0.6Cu is available from the indium Corporation as our Indalloy
252.
There are a number of tin/silver/copper alloys, and as the technical
differences between most of them are somewhat notional, we naturally would
prefer to single up to just one. This is Indalloy 241 (95.5Sn/3.8Ag/0.7Cu).
Perhaps this is what Ioan has understood to mean not available (assuming he
contacted us)
Regards
Mike Fenner
Applications Engineer, European Operations
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Leadfree: www.Pb-Free.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Tempea, Ioan
Sent: Friday, March 07, 2003 5:19 PM
To: [log in to unmask]
Subject: Re: [TN] Leadfree alloy supplier
It would be interesting to have the information sent to the Technet.
This is the alloy that NEMI recommends and a few months ago, when I tried to
find it, no major paste manufacturers had it. Do they feel like moving
towards this alloyÉ
Regards,
Ioan
> -----Original Message-----
> From: Gerard O'Brien [SMTP:[log in to unmask]]
> Sent: Friday, March 07, 2003 11:30 AM
> To: [log in to unmask]
> Subject: [TN] Leadfree alloy supplier
>
> I am looking for a supplier of the following lead free alloy -
> 95.5Sn/3.9Ag/0.6Cu.
>
> You can contact me off line.
>
> Regards
>
> Gerard O'Brien
> Photocircuits Corporation
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|