Get the IPC/WHMA-A-620 for cable and wire acceptance criteria.
Section 4 states Stranded wires shall be tinned prior to forming for attachment to solder terminals. (Stranded wires for attachment to crimp terminals shall not be tinned see 5 crimp terminals).
Section 5 states that conductors should not be tinned prior to termination, unless otherwise specified.
Kat
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
<!DOCTYPE HTML PUBLIC "-//W3C//DTD HTML 4.0 Transitional//EN">
<HTML><HEAD>
<META http-equiv=Content-Type content="text/html; charset=iso-8859-1">
<META content="MSHTML 6.00.2715.400" name=GENERATOR></HEAD>
<BODY style="MARGIN-TOP: 2px; FONT: 8pt MS Sans Serif; MARGIN-LEFT: 2px">
<DIV><FONT size=1>Get the IPC/WHMA-A-620 for cable and wire acceptance
criteria. </FONT></DIV>
<DIV><FONT size=1></FONT> </DIV>
<DIV><FONT size=1>Section 4 states Stranded wires shall be tinned prior to
forming for attachment to solder terminals. (Stranded wires for attachment to
crimp terminals shall not be tinned see 5 crimp terminals).</FONT></DIV>
<DIV><FONT size=1></FONT> </DIV>
<DIV><FONT size=1>Section 5 states that conductors should not be tinned
prior to termination, unless otherwise specified.</FONT></DIV>
<DIV> </DIV>
<DIV><FONT size=1>Kat</FONT></DIV></BODY></HTML>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|