Glenn,
Try to check IPC-4552 (new standard for ENIG).
Rey Degollado
QM Asst. Supervisor
Daeduck Phils., Inc.
PEZA, Rosario, Cavite, Phils.
Office : (046) 437-0741~48 loc. 293,292
Mobile : 09196671489
Glenn Pelkey
<glenn.r.pelkey@M To: [log in to unmask]
AXTEK.COM> cc:
Sent by: TechNet Subject: [TN] Electroless Gold Industry
<[log in to unmask]> Standard
03/25/2003 08:44
AM
Please respond to
"TechNet E-Mail
Forum."; Please
respond to
glenn.r.pelkey
Hi folks,
Anyone know what industry standard to specify with respect to
Electroless Gold? ASTM, IPC, etc?
Thanks,
Glenn
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|