Yes, now you are getting picky ;~) Do you have a copy of IPC-D-279?
Section 3.5 Solder Joint Reliability, specifically 3.5.1.3 Solder Joint
Height seems to be the variable you are asking about. It is part of the
prediction equations A-3 and A-4 in the Design Guidelines. I have not
seen these translated into DFR rules. I think the other variables you
mentioned would exert too much of an influence to make any hard and fast
rules. Flexible rules . . . Sounds like Philadelphia traffic laws.
Werner?
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
> Sent: Thursday, March 20, 2003 1:31 PM
> To: [log in to unmask]
> Subject: Re: [TN] SMT Component Standoffs
>
>
> Thanks, Guy, BUT this has to do with cleaning rather than
> mechanical reliability.
> Bev
> --------------------------
> Sent from my BlackBerry Wireless Handheld (www.BlackBerry.net)
>
>
> -----Original Message-----
> From: Guy Ramsey <[log in to unmask]>
> To: 'TechNet E-Mail Forum.' <[log in to unmask]>; Bev Christian
> <[log in to unmask]>
> Sent: Thu Mar 20 13:17:55 2003
> Subject: RE: [TN] SMT Component Standoffs
>
>
> There is help in IPC-SM-782A section 3.6.1.7 Component Stand
> Off Height for Cleaning and the associated table 3-7. The
> stand off recommendation varies with the component size. For
> example small component < 3mm x 3mm stand off > 0.05 mm. A
> large component 50mm x 50 mm stand off > 0.5 mm.
>
> > -----Original Message-----
> > From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
> > Sent: Thursday, March 20, 2003 12:56 PM
> > To: [log in to unmask]
> > Subject: [TN] SMT Component Standoffs
> >
> >
> > TechNetters,
> > When I was at a former employer there was a minimum stand off
> > in the company specs. I have forgotten what that was. Now I
> > know that it can/should be different based on the solder, use
> > environment, pad sizes and lead/termination materials, but I
> > was wondering if anyone would be willing to share what they
> > have on the subject. I am particularly interested in land
> > grid array devices, if I may be so bold as to be picky. :)
> > Thanks in advance.
> > Bev Christian
> > Research in Motion
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a free service by IPC using
> > LISTSERV 1.8e To unsubscribe, send a message to
> > [log in to unmask] with following text in the BODY (NOT the
> > subject field): SIGNOFF Technet To temporarily halt or
> > (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE
> > mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest Search the archives of
> > previous posts at: http://listserv.ipc.org/archives Please
> > visit IPC web site http://www.ipc.org/html/forum.htm for
> > additional information, or contact Keach Sasamori at
> > [log in to unmask] or 847-509-9700 ext.5315
> > -----------------------------------------------------
> >
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using
> LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with
> following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send
> e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail
> to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|