Hi Marie,
Being a Contract Manufacturer , we had to deal with an equal design.
The board was also 2.3mm and via-holes were used as testpads.
Using the via's as testpads was a disaster. It didn't work.
We tried to cover the via's with solderpaste but that didn't give any
improvement.
The holes were just too big. (forgive me , I don't remember the size).
And solderpaste disapeared in the hole.
Until now this issue still isn't solved.
We decided not to accept any similar design until we find a adequate
solution for testvia's.
So Marie , I can't help you but perhaps you can use this as feedback to your
customer.
Good luck
Jowan Iven
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Marie-Elisabeth MAGNIN
Sent: vrijdag 14 maart 2003 11:02
To: [log in to unmask]
Subject: Re: [TN] 2.3mm thick PCB and BGA
Hi Peter
Thanks for your quick answer. Here are some further explanations :
application is avionics ! I also have concerns about copper plating in the
hole. This is the first point I told my customer. We just met a similar
problem last week on a 1.6mm thick PCB and 0.2mm via holes, the copper layer
broke when changing wrong BGA's.
to save place, the idea is to use via pads as test pads : via holes should
not be epoxy filled, but filled with a conductive material to create a
"large" test pad to contact on the test fixture (large despite a round pad
of 0.6mm diameter). Unfortunatly, it cannot be filled during wave soldering
(the process will only be reflow).
ME Magnin
mailto:[log in to unmask]
http://www.firstec.ch
---------------------------------------------------
========================================================================
DISCLAIMER:
The information contained in this communication is confidential and may be legally privileged.
It is intended solely for the use of the individual or entity to whom it is addressed and others
authorized to receive it. If you are not the intended recipient, you are hereby notified that any
disclosure, copying, distribution, or taking any action in reliance of the contents of this information
is strictly prohibited and may be unlawful. Stork is neither liable for the proper and complete
transmission of the information contained in this communication nor for any delay in its receipt.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|