TECHNET Archives

March 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset="us-ascii"
Sender:
Subject:
From:
Date:
Tue, 11 Mar 2003 11:20:27 -0600
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (98 lines)
Tom,
I think you are missing something.  In both scenarios you describe, you
have USED two different types of fluxes on one assembly but have not MIXED
two different kinds of fluxes on one assembly.  When you wash the water
soluble flux, it is gone (well, in theory at least), and so you are not
mixing fluxes.

I would also caution those who might think that when you mix a no-clean and
a water soluble flux that a cleaning operation removes the water soluble
flux.  Not the case.  When you mix chemistries, you have an amalgam which
is often very resistant to cleaning, and still corrosive.

Doug Pauls




                      "Tom Parkinson -
                      Quality System           To:       [log in to unmask]
                      Manager -                cc:
                      WinTronics, Inc."        Subject:  Re: [TN] Mixing fluxes - more
                      <tomp@WINTRONICSI
                      NC.COM>
                      Sent by: TechNet
                      <[log in to unmask]>


                      03/11/2003 10:39
                      AM
                      Please respond to
                      "TechNet E-Mail
                      Forum."; Please
                      respond to "Tom
                      Parkinson -
                      Quality System
                      Manager -
                      WinTronics, Inc."






I've read the recent questions and information concerning mixing of
fluxes.  I agree - do not mix flux types when soldering.  However,
here's one for you that can be looked at from a couple of angles....

1. I build a board - wave solder using washable flux.  Flux is
activated, does it's thing, and board is soldered.
2. Water Wash and Dry the board. All washable flux residue is gone.
3. Add a couple of more components that CANNOT be washed (water will
enter the component and ruin it), using NO-CLEAN.
4. Board is done.

Technically, I have used 2 types of fluxes on one assembly....

Another scenario:
1. Board (described above) is finished.  But, fails test - I find a bad
component...
2. I have to use NO CLEAN to replace the component because I cannot
water wash the board (remember the other components that cannot be
subjected to water wash..)
3. Board is done. Passes test - finished.

Again - Technically, I have mixed fluxes on the same assembly.

In the above description, I do not see a problem - or am I missing
something?


Thanks,
Tom

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2