You might look at the solderpaste you're using. We found significant
differences in voiding with water soluble pastes. I suspect there are
similar differences with no-cleans.
Rick Thompson
Sr. SMT Process Engineer
SMTEK International, Inc.
+1 (805) 532-2800
[log in to unmask]
===== Original Message from [log in to unmask] (TechNet E-Mail Forum.) at
3/11/03 5:14 am
>Hi,
>
> We experience some void in BGA. We try different paste and profile but
>nothing seem to eliminate those void. We try something, we took a BGA and
>put only flux on the ball( Flux 297DX from AIM) and we didn't see any
>voiding after that...
>
> We use stencil of .006mil, and .005mil of thickness, and we had some
>medium to large void
>
> We also try a .004 stencil ( like a mini-stencil) where we put some paste
>and we had some little BGA.
>
> My question is, could the paste and the ball of the BGA could not be
>compatible( we use a no clean solder paste, 63/37, our Solder ball under BGA
>are also 63/37).
>
> Or is the stencil thickness is very important??
>
> We use a 10% reduction on the stencil whti round pad
>
>Thanks You
>
>Yannick Brisson
>============================
>Technicien SMT
>Technician SMT
>M2S Électronique
>2855, Rue de Celles
>Québec, Québec
>G2C 1K7
>Téléphone: (418) 842-1312 Ext: 264
>Télécopie: (418) 842-0123
>[log in to unmask]
>============================
>
>---------------------------------------------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|