TECHNET Archives

February 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Rey Degollado <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Sat, 8 Feb 2003 16:03:13 +0800
Content-Type:
text/plain
Parts/Attachments:
text/plain (180 lines)
Gerard,

Does this new IPC specification covers other finishes such as Immersion
Tin, Silver etc? I ask because we will be starting to produce this types of
PCBs.

Thanks.

Rey Degollado
Quality Management
Daeduck Phils., Inc.




                    Gerard O'Brien
                    <gobrien@PHOTOCIR        To:     [log in to unmask]
                    CUITS.COM>               cc:
                    Sent by: TechNet         Subject:     Re: [TN] Evaluating ENIG finish
                    <[log in to unmask]>


                    02/07/2003 09:59
                    PM
                    Please respond to
                    "TechNet E-Mail
                    Forum."; Please
                    respond to Gerard
                    O'Brien






Ervin - get yourself a copy of the new IPC4552 specification covering ENIG.
Use this document to specify the ENIG finish for your PWB's.





Regards





Gerard O'Brien


Co-chairman of 4552





     -----Original Message-----
     From: Ervin Weisz [mailto:[log in to unmask]]
     Sent: Thursday, February 06, 2003 5:43 PM
     To: [log in to unmask]
     Subject: [TN] Evaluating ENIG finish





     Hello Everyone,


     I wish to present you with an issue that has troubled me for quite a
     while.





     We have been ordering more and more PCBs with ENIG finish and are
     generally pleased - it's flat, it solders nicely and the products seem
     to be O.K.


     However, on the other hand - we are very well aware of problems
     associated with ENIG, i.e - the "black pad" phenomena - solder joints
     cracking, components actually "popping off" and other "goodies".





     I am looking for good means to evaluate my ENIG finished boards,
     before I waste a considerate amount of money while trying to assemble
     them. Luckily for us, our manufacturer seems to understand our dilemma
     and is very willing to cooperate with us on performing any in-process
     or final test that we specify.





     So, here's the catch: what do I specify ?





     Assume that you could ask for anything (within reason, of course) -
     what tests would you ask your manufacturer to perform to assure you
     that he will give you high quality ENIG finish, good solderability,
     durable, long life solder joints, etc.?





     Thank you in advance,





     Yehuda E. Weisz


     +(972)-3-6342045


     +(972)-53-556897








     Do you Yahoo!?
     ---------------------------------------------------
     Technet Mail List provided as a free service by IPC using LISTSERV
     1.8e
     To unsubscribe, send a message to [log in to unmask] with following text
     in the BODY (NOT the subject field): SIGNOFF Technet
     To temporarily halt or (re-start) delivery of Technet send e-mail to
     [log in to unmask]: SET Technet NOMAIL or (MAIL)
     To receive ONE mailing per day of all the posts: send e-mail to
     [log in to unmask]: SET Technet Digest
     Search the archives of previous posts at:
     http://listserv.ipc.org/archives
     Please visit IPC web site http://www.ipc.org/html/forum.htm for
     additional information, or contact Keach Sasamori at [log in to unmask] or
     847-509-9700 ext.5315
     -----------------------------------------------------
     Yahoo! Mail Plus - Powerful. Affordable. Sign up now


---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2