Hello T'Netters,
Recently our lab provided qualification testing of a board house for an OEM.
The OEM requires surface copper of a particular thickness (e.g., 2.8 - 3.6
mil).
We provided measurements from a number of cross-sections.
We measured both PTH copper dimensions and, elsewhere on the board,
provided typical surface copper measurements. The stack-up measurments
of the PTH's evidenced slightly less than the minimum surface copper
thickness
mandated by the OEM. So, the OEM rejected the board house.
Is it fair to use surface copper measurements near PTH's to characterize the
copper thickness of PWB's? Could subsequent processing in the absence
of solder resist result in lowered copper thickness? Does any military or
industry specification mandate or even suggest appropriate areas for surface
copper measurement?
TIA for any insights offered.
Mike Simms
Chemist
Trace Laboratories - Central
1150 West Euclid Avenue
Palatine, IL 60067
phone 847-934-5300
fax 847-934-4600
www.tracelabs.com
Notice: This message is confidential and intended for the private use of
the addressee only.
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|