Rick
We're assembling some Teflon boards right now with no issues.
The boards we build require a slightly hotter profile to see sufficient
time above 183, but, your boards may be different.
My only word of caution is hand soldering. Be careful not to lift pads
as rework may not be as easy with the traditional FR4's.
-Carrie
-----Original Message-----
From: Rick Thompson [mailto:[log in to unmask]]
Sent: Monday, February 24, 2003 10:06 AM
To: [log in to unmask]
Subject: [TN] Teflon Substrate Processing?
Hi,
We have a customer using Teflon substrates (I don't have details yet on
exact material) and I'm hoping someone can give me some feedback on any
special processing that might be needed working with these boards?
Additional baking, reflow profiles, washing, etc?
Thanks in advance.
Rick Thompson
Sr. SMT Process Engineer
SMTEK International, Inc.
+1 (805) 532-2800
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|