>The customer is looking for a statement from us about reliability issues if
>the go to lead free (15 year warranties).
>His concern is that the results on the test board's are not fully comparable
>to the reality.
>
>What is your recommendation:
>Which test should be used Twist and Bending, T cycles, T shock....
***We do not have a creep-fatigue model or acceleration factors for
LF-solders. Thus, the only way to warrant 15 years is to T-cycle according to
SM-785 and IPC-9701 relatively close to the T-extremes experienced in the
field. LF-solders have an even more complex creep-fatigue behavior than Sn/Pb
solders.
>What is the most critical think according to your opinion (brittle fracture
of BGA solder joints because of mechanical bending ?)
*** If the BGA interfaces are the weak link yes, but it depends on the
largest CTE-mismatch in you PCA.
>Would you change land and stencil design?
***I have seen no indication for this.
>Which standards would you use to qualify the PCBA for the product?
***IPC-9701
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|