I have seen supplier data, with reliability test info, that supported this.
They did a good job with the assessment, but personally, I still don't think
it's a smart thing to do.  In addition to lack of adhesion, the galvanic
series shows an unacceptable couple between silver and tin.  Granted, it's
hermetic.  But, the assembly time before it goes into the hermetic package
needs to be considered.

For prototyping, there may be a need to qualify a design in a hurray, and it
may be the only option.  But, definitely not for production quantities.

Glenn

-----Original Message-----
From: Creswick, Steven [mailto:[log in to unmask]]
Sent: Tuesday, February 11, 2003 6:28 AM
To: [log in to unmask]
Subject: Re: [TN] conductive epoxy


James,

I would prefer NOT to use any adhesive for a tin plated, or 'tinned' (solder
coated) temination in that temperature range.

My experience is that it will soon mechanically fall apart, resulting in
electrical discontinuity as well.

See what everyone else says.

Steven Creswick - Gentex Corporation

-----Original Message-----
From: James TerVeen [mailto:[log in to unmask]]
Sent: Tuesday, February 11, 2003 8:47 AM
To: [log in to unmask]
Subject: [TN] conductive epoxy


I have a customer who wants to epoxy a multilayer capacitor to the
following and is not sure what conductive epoxy would be the best.     The
terminations on the capacitor is nickel with a tin overplate.
Any suggestions.

The capacitors are to be installed in hermeticly sealed  hybrid oscillator
circuits.
The internal enviornment is either a vacuum or backfilled nitrogen.
The substrates are Alumina  and the metalization is gold or silver.
The ambient temperature range is from -55 deg.c. to +125 deg.c.

Thanks

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2