Hi Mike,
>Is it fair to use surface copper measurements near PTH's to characterize the
copper >thickness of PWB's?
ANSWER: No, it is much more technically important and accurate to measure the
plating thickness in the PTH.
>Could subsequent processing in the absence of solder resist result in
lowered copper >thickness?
ANSWER: Yes, it certainly will.
>Does any military or industry specification mandate or even suggest
appropriate areas for >surface copper measurement?
ANSWER: No, measurements are to be inside the PTH--see for instance IPC-D-279.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|