Nee how Wee Mei,
The shape of a solder joint does have an effect on reliability, but it is of
2. order. Satoh of Hitachi did work on this and published a paper --in IEEE
Transactions, I think-- where he changed solder ball geometry from suat ball
to hour-glass by changing the the distance between
PWB and component. The increase in fatigue life came mostly, but not all,
from the increased solder joint height.
Another piece of evidence is that with balls the failure mode in near the
interface, for column-like geometries the failure mode is frequently away
from the interface.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|