We currently only use the blue water washable markers. I have seen boards with marks come from storage after 6+ months. They washed off fine with now visible effect. The red solvent markers sometimes stained certain materials but this did not seem to be time dependent but material. One caution, the water washable can stain if exposed to some solvents like xylene.
-----Original Message-----
From: Larry Koens [mailto:[log in to unmask]]
Sent: Friday, February 28, 2003 9:08 AM
To: [log in to unmask]
Subject: [TN] Fluxmarker
We use the water soluble fluxmarkers made by Sanford. I've been trying to find out how long this marker can remain on the PCB before washing is required. Does anyone else use these markers? How long do you leave the markings on your assembly before washing?
-Larry Koens-
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|