I have yet to find a real relevance for the equivalence factor - it was
used to indicate relative sensitivity of measuring equipment compared to
the original manual method of determining board cleanliness. As long as you
test the linearity of your contamination measuring equipment (i.e. 1:1
reading:salt put in), or determine the drift, you will know what your
machine is capable of in absolute terms.
It's my conclusion that the equivalence factor is an unnecessary red
herring, but I still worry about it and would love to be convinced about
how it fits into the equation.
Peter
"d. terstegge" <[log in to unmask]> 28/02/2003 12:54 AM
Sent by: TechNet <[log in to unmask]>
Please respond to "TechNet E-Mail Forum."; Please respond to "d. terstegge"
To: [log in to unmask]
cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Subject: Re: [TN] Ionic Equivalence
Hi Charlie,
I had a question about this at the end of September last year and
received many answers (search for the thread "Ionograph measurements").
For the Omegameter 600 the equivalence factor is 1.39.
I will send you some relevant documentation off-Technet, as attachments
are stripped by the Technet-server.
Daan Terstegge
Thales Communications
Unclassified mail
Personal Website: http://www.smtinfo.net
>>> [log in to unmask] 02/27/03 05:16pm >>>
I need to meet a Bellcore requirement on an assembly of
6.45ugrams/sq.in.
(Based on the pwb surface area)
The assembly has 633.5 sq.in. surface area.
The customer has supplied me with documentation from;
Physical Design and Manufacture of Telecommunications Products PWB
Assembly
Requirements, GR-78-CORE, Issue 1, Sept 1997. Section 7.1.3.9
I have an Omegameter 600. Is there an equivalence factor, etc? Or is it
a 1
to 1 deal?
Thanks in advance.
Charlie
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV
1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|