Hi Mike,
You remind me of someone told me that there is reflow machine that provide short liquidus time. I do not recall the brand name of the machine, but I understand it is an European machine.
I see the reflow profile is having around 20 seconds liquidus time.
Poh
--- Mike Fenner <[log in to unmask]> wrote:
> Keeping the time over liquidus as short as possible and rapid
> cooling as
> possible will help, subject to the possibilities of your system
>
> Regards
>
> Mike Fenner
>
> Applications Engineer, European Operations
> Indium Corporation
> T: + 44 1908 580 400
> M: + 44 7810 526 317
> F: + 44 1908 580 411
> E: [log in to unmask]
> W: www.indium.com
> Leadfree: www.Pb-Free.com
>
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Morse, Carrie
> Sent: Thursday, February 27, 2003 3:57 PM
> To: [log in to unmask]
> Subject: Re: [TN] : Shining smooth solder joint on ENIG or Gold
> plating
> Board.
>
>
> Poh,
> Although shiny joints are not an IPC/J-STD requirement, you can
> minimize
> dullness by using nitrogen in your oven, or, by changing solder
> pastes.
> Some pastes provide for shinier joints than others. But again,
> shininess is
> not a requirement.
>
> -Carrie
>
> -----Original Message-----
> From: Poh Kong Hui [mailto:[log in to unmask]]
> Sent: Thursday, February 27, 2003 7:18 AM
> To: [log in to unmask]
> Subject: [TN] : Shining smooth solder joint on ENIG or Gold plating
> Board.
> Importance: High
>
>
> Hi Technetters,
>
> Can someone advise me how to get a good smooth shining solder joint
> on the
> ENIG board or board with gold plate SMT pads.
>
> As I can understand that board subjected to reflow soldering, the
> solder
> joint tends to look dull and not so smooth joint. But, is there any
> way to
> get a good shining joint.
>
> Thanks.
>
> Poh
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV
> 1.8e
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail
> to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700
> ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV
> 1.8e
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail
> to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700
> ext.5315
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV
> 1.8e
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|